KINGARC E309L
Dissimilar joints between stainless steels and low alloy or carbon steels · SS piping in refineries, oil and gas industries, chemical plants · Welding of AISI 309, 309L type steels.
Specification — the value specified for the gradeTypical — typical values for the grade, as published by PWL
Chemical composition of undiluted weld metal, %
| C | Mn | Si | S | P | Ni | Cr | Mo | Cu | |
|---|---|---|---|---|---|---|---|---|---|
| Specification | 0.04 max | 0.50 – 2.50 | 1.00 max | 0.030 max | 0.040 max | 12.0 – 14.0 | 22.0 – 25.0 | 0.75 max | 0.75 max |
| Typical | 0.03 | 1.5 | 0.45 | 0.02 | 0.02 | 13.1 | 23.6 | 0.22 | — |
Swipe sideways for all columns →
Mechanical properties of all weld metal — as welded
| UTS, MPa | Elongation, % | |
|---|---|---|
| Specification | 520 min | 30 min |
| Typical | 580 | 36 |
Swipe sideways for all columns →
Welding current — by diameter and length
| Size | Welding current, A |
|---|---|
| Ø 2.50 × 350 mm | 50 – 80 |
| Ø 3.15 × 350 mm | 80 – 100 |
| Ø 4.00 × 350 mm | 110 – 140 |
Swipe sideways for all columns →
Re-drying
250 – 300 °C for minimum 1 hr.
Same alloy for TIG welding
Packing
Branded KINGARC carton, marked with grade and size. Packaging specification →