Flux–wire selector
| Flux | Wires | Classification | Suited to |
|---|---|---|---|
| PWL 5101 | EL8 · EM12K | F7AZ-EL8 · F7AZ-EM12K | Boiler water walls at high speed · boilers, pressure vessels, ships |
| PWL 6101 | EH10K · EH12K | F7A6 / P6-EH10K / EH12K | Low alloy and high strength steel, 2 to 6 wires |
| PWL 7101 | EM12K · EH14 · EA2 | F7A4-EM12K · F7A4-EH14 · F8A2-EA2 | Oil and gas pipeline steel · wind mill towers · bridges |
| PWL 7101G | EM12K · EA2 · EA2TiB | F7A4-EM12K · F8A2-EA2 · F9A2-EA2TiB | Straight seam and spiral pipe to X70 / X80 · up to 4 arcs |
| PWL 8101M | EL8 · EM12K | F7AZ-EL8 · F7A0-EM12K | Spiral pipe for water pipelines · suits multiple-wire welding |
| PWL 8101 | EM12K · EH14 | F7A2-EM12K · F7A4-EH14 | Boiler pressure vessels · ships · bridges · oil transmission lines |
| PWL 9101 | EM12K · EG · EA2TiB | F7A4-EM12K · F9A4-EG · F9A2-EA2TiB | Nitrogen-limiting seam welding of pipe · up to 6 arcs · X60 – X80 |
Swipe sideways for all columns →
How to read a designation — F7A2-EM12K
F7A2–EM12K
F submerged arc welding flux. 7 the strength of the weld metal — 70 to 95 ksi tensile, 58 ksi minimum yield, 22 % minimum elongation. A tested as welded; P would mean after post-weld heat treatment. 2 the impact test temperature — 27 J at −20 °C. EM12K the wire electrode the flux was classified with.
Impact designator — AWS A5.17M / A5.23M
| Digit | Test temperature | Minimum energy |
|---|---|---|
| Z | No impact requirement | — |
| 0 | 0 °C | 27 J |
| 2 | −20 °C | 27 J |
| 4 | −40 °C | 27 J |
| 6 | −60 °C | 27 J |
The digits used across the PWL flux range, with the test temperature in °C as per AWS A5.17M / A5.23M.
Swipe sideways for all columns →

A grade that is not listed?
PWL developed EA2TiB and S3TiB wires — previously imported — for API-grade pipe, together with a flux engineered for API projects. For a chemistry or a flux–wire combination not shown here, please contact us.