Specification — the value specified for the gradeTypical — typical values for the grade, as published by PWL
AWS A5.18 grades — chemical composition of wire, %
| AWS | C | Mn | Si | S | P | Cu coating % | |
|---|---|---|---|---|---|---|---|
| PWL MIG 1 specification | ER70S-2 | 0.07 max | 0.90 – 1.40 | 0.40 – 0.70 | 0.035 max | 0.025 max | 0.50 max |
| PWL MIG 1 typical | ER70S-2 | 0.06 | 1.33 | 0.67 | 0.015 | 0.01 | 0.20 |
| PWL MIG 2 specification | ER70S-6 | 0.06 – 0.15 | 1.40 – 1.85 | 0.80 – 1.15 | 0.035 max | 0.025 max | 0.50 max |
| PWL MIG 2 typical | ER70S-6 | 0.09 | 1.48 | 0.85 | 0.015 | 0.01 | 0.20 |
Swipe sideways for all columns →
AWS A5.28 grades — chemical composition of wire, %
| AWS | C | Mn | Si | S | P | Mo | Cu coating % | |
|---|---|---|---|---|---|---|---|---|
| PWL MIG 3 specification | ER80S-G | 0.06 – 0.14 | 1.30 – 2.10 | 0.40 – 1.15 | 0.035 max | 0.025 max | 0.60 max | 0.50 max |
| PWL MIG 3 typical | ER80S-G | 0.09 | 1.80 | 0.63 | 0.008 | 0.009 | 0.52 | 0.20 |
| PWL MIG 4 specification | ER90S-G | 0.07 – 0.12 | 1.60 – 2.10 | 0.50 – 0.80 | 0.025 max | 0.025 max | 0.40 – 0.60 | 0.50 max |
| PWL MIG 4 typical | ER90S-G | 0.10 | 1.95 | 0.67 | 0.006 | 0.009 | 0.55 | 0.20 |
Swipe sideways for all columns →
Mechanical properties of weld metal
| UTS, MPa | YS 0.2 %, MPa | Elongation, % | CVN at −30 °C, J | |
|---|---|---|---|---|
| PWL MIG 1 specification | 490 min | 400 min | 22 min | 27 |
| PWL MIG 1 typical | 520 | 430 | 27 | 85 |
| PWL MIG 2 specification | 490 min | 400 min | 22 min | 27 |
| PWL MIG 2 typical | 550 | 450 | 28 | 90 |
| PWL MIG 3 specification | 550 min | 500 min | 20 min | 27 |
| PWL MIG 3 typical | 620 | 520 | 24 | 78 |
| PWL MIG 4 specification | 620 min | 540 min | 17 min | 27 |
| PWL MIG 4 typical | 670 | 590 | 25 | 80 |
Swipe sideways for all columns →
Classification, shielding gas and use
PWL MIG 1AWS A5.18 ER70S-2 · CO₂Structural, pressure vessel and boiler work involving unalloyed and micro-alloyed structural steels.
PWL MIG 2AWS A5.18 ER70S-6 · CO₂Unalloyed construction steels, shipbuilding steels and low alloyed, general purpose C-Mn steels of increased strength. 0.80 – 1.60 mm for fabrication; 2.50 – 4.00 mm for tack welding in pipe application.
PWL MIG 3AWS A5.28 ER80S-G · CO₂ and Ar + CO₂All position welding with a smooth, stable, low-spatter arc. Joining carbon steel and low alloy steel.
PWL MIG 4AWS A5.28 ER90S-G · CO₂ and Ar + CO₂HSLA and creep resisting steels — higher strength welds and construction equipment. 1.20 – 1.60 mm; larger diameters by prior agreement.