Specification — the value specified for the gradeTypical — typical values for the grade, as published by PWL
Chemical composition, %
| C | Mn | Si | S | P | Ni | Cr | Mo | Cu | |
|---|---|---|---|---|---|---|---|---|---|
| Specification | 0.03 max | 1.00 – 2.50 | 0.30 – 0.65 | 0.030 max | 0.030 max | 11.0 – 14.0 | 18.0 – 20.0 | 2.0 – 3.0 | 0.75 max |
| Typical | 0.027 | 1.8 | 0.45 | 0.02 | 0.02 | 11.5 | 18.5 | 2.5 | — |
Swipe sideways for all columns →
Mechanical properties of all weld metal — as welded
| UTS, MPa | Elongation, % | |
|---|---|---|
| Specification | 490 min | 30 min |
| Typical | 560 | 35 |
Swipe sideways for all columns →
Sizes, current and gas
1.6 · 2.0 · 2.4 · 3.15 · 4.0 mm × 1000 mm · DCEN, all positions · argon 10 to 15 l/min.
Same alloy as a covered electrode
Packing
Cut lengths in a sealed tube, 5 kg. AWS grade embossed on each rod. Packaging specification →